Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Radici Heraflex® A 57-41-90 TPS-SEBS Thermoplastic Elastomer Shore hardness: 57A (3s)Good price / compression set ratioApplication examples: sealing for spoutsInformation provided by Radici group. |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D 792 |
Karina E550D06/957 Blue PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D 792 |
Karina TR-607D48/1-Y-IS-BZ Black PVC Compound Heavy metal free PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ISO 1183 |
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Shin-Etsu Silicones X-30-783U Silicone Elastomer ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Teknor Apex APEX® 90-A471R-6-NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 94-A0098C-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | DCBP Cure |
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer ShinEtsu KE5551 U is a nominal 50 Durometer base which offers high tensile and tear strengths. Its excellent processing characteristics make it suitable for molding, extrusion and calendaringProduct.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE DescriptionPOLYBATCH® 40442 is a light blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40442 is typical.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE DescriptionPOLYBATCH® 40442 is a light blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40442 is typical.. |
|||
Specific Gravity | 1.17 g/cc @Temperature 25.0 °C |
1.17 g/cc @Temperature 77.0 °F |
|
Dow Corning D94-20P A&B KIT Two-part, 1:1 ratio, addition cure silicone elastomer for automated assembly of integrated compression sealsInformation provided by Dow Corning |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
AlphaGary Garaflex™ X 95-759 B-1 Vinyl Thermoplastic Elastomer Garaflex™ is a vinyl based thermoplastic elastomer used mostly in footwearSlaughter House |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D792 |
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
PolyOne Synprene® IT 37-033 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A therm.. |