| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Elastomer, for Thermal Management | 
| Manufacturer | Dow Corning | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Dow Corning D94-20P A&B KIT.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.17           g/cc @Temperature 25.0 °C | 1.17           g/cc @Temperature 77.0 °F | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 21 | 21 | |
| Tensile Strength, Ultimate | 5.900 MPa | 855.7 psi | |
| Elongation at Break | 925 % | 925 % | |
| Modulus of Elasticity | 0.000390 GPa | 0.0566 ksi | 150% elongation | 
| Tear Strength | 231 kN/m | 1320 pli | |
| Compression Set | 36 % | 36 % | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Flash Point | >= 100 °C | >= 212 °F | closed cup | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Cure Time | 2.75           min @Temperature 115 °C | 0.0458           hour @Temperature 239 °F | |
| Shelf Life | 12.0 Month | 12.0 Month | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Mix Ratio (X:1) | 100 | Base to Catalyst ETN |