Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Polymax® Maxelast® P2775 TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Network Polymers SAN 290 High Flow Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Palm Labs Adhesives TURBO-LOCK SERIES 11-OR Anaerobic Thread Locking Compound TURBO-LOCK 11-OR SERIES is a fast curing, BLUE, removable, medium strength, oil resistant, primerless, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Solvay Engineered Polymers SEQUEL® 1733HI Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1733HI engineered polyolefin is designed for large, painted automotive exterior applications that require dimensional stability over a broad temperature range. This material e.. |
|||
Specific Gravity | 1.07 - 1.11 g/cc | 1.07 - 1.11 g/cc | |
LG Chemical CP-RS Polycarboxylic Copolymer Description: CP-RS is the main raw material for concrete admixture, which improves water reducing ability of high early strength concrete. CP-RS exhibits superior property of early strength developm.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Momentive Performance Materials TUFELâ„¢ II 94205 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM-D792 |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM 792 |
Multibase Multi-Flex® A 4001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information pro.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM 792 |
Multibase Multi-Flex® A 5904 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Spartech Royalstatâ„¢ R675 PS Alloy Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | 23°C; ASTM D792 |
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Teknor Apex Tekbond® TB 1176A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Chase Plastics CP Pryme® NN200STL (DAM) Nylon 66, Super-Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange 1770E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1770E is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1770E is .. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Zylog Hipolyene® 1532 MS Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Dow Corning Z-1219 DIMETHYLDICHLOROSILANE Dimethyldichlorosilane (ch3)2sicl2 - synthesis of silanes, silicones; hydrophobic treatment; pyrolysis to si-c coatings; protective group in organic synthesis.Information provided by Dow Corning |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Diamond Polymers ABS 4001H3F Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ISO 1183/1 |
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | 23/23°C; ASTM D792 |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |