Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.01 g/cc | 1.01 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Polymax® Maxelast® P3885M TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM 792 |
Multibase Nylex™ 2185 FR Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Specific Gravity | 1.01 - 1.03 g/cc | 1.01 - 1.03 g/cc | |
Michelman® GlossCoat™ 100 BL Preprint varnish Description: Water based, nonskid preprint varnish for porous substratesUsage: GlossCoat™ 100BL is a fully formulated, flexo appliable nonskid coating designed for kraft, mottled and bleached s.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4855A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-2563A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4020 Concentrate Based In Polyethylene DescriptionPOLYBATCH® Blue 4020 is a blue color concentrate based in polyethylene. This concentrate was designed to provide intense blue color in polyolefin film and molding applications. POLYBA.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Trelleborg R506 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4020 Concentrate Based In Polyethylene DescriptionPOLYBATCH® Blue 4020 is a blue color concentrate based in polyethylene. This concentrate was designed to provide intense blue color in polyolefin film and molding applications. POLYBA.. |
|||
Specific Gravity | 1.01 g/cc @Temperature 25.0 °C |
1.01 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles .. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | Part B |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Diamond Polymers SBS 1031 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Specific Gravity | 1.01 - 1.08 g/cc | 1.01 - 1.08 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D-792 |
Chevron Phillips K-Resin® KR03BR SBC