Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Laurel BioComposite, Ltd.
Trade Name Bio-Res™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteristics of the end product. Bio-Res is created from a bio-based feedstock, initially distillers grains, a by-product of the ethanol process. The feedstock undergoes a proprietary process which creates a product for inclusion in thermoplastics. Bio-Res can be delivered as a fine powder or in pellet form.Data is for a 20% filler loading on injection molded HDPE samples.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
Water Absorption 0.27 %

@Time 86400 sec
0.27 %

@Time 24.0 hour
Immersion
Linear Mold Shrinkage 0.03 cm/cm
0.03 in/in
Mechanical Properties Metric English Comments
Tensile Strength 15.9 MPa
2300 psi
ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Flexural Strength 29.6 MPa
4300 psi
ASTM D790
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Izod Impact, Notched 0.37 J/cm

@Thickness 3.17 mm
0.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Processing Properties Metric English Comments
Die Temperature 193 - 204 °C
380 - 400 °F
Extrusion
Melt Temperature 177 - 191 °C
350 - 375 °F
Extrusion
177 - 193 °C
350 - 380 °F
Injection
Mold Temperature 32 - 65.6 °C
90 - 150 °F
Injection
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.0 hour
Extrusion or Injection