Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.905 g/cc | 0.905 g/cc | 23/23°C; ASTM D792 |
M. Holland Company PP200 Polypropylene Homopolymer High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3575CC Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblo.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4720XWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 502HC Thermoforming Polypropylene Homopolymer Disposable cupware and dishware; High-stiffness parts; Hot packaging.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |