Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE) Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE) Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT226 Thermoplastic Elastomer (TPE) Versaflex™ HC MT226 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT226 has been specially formulated to be free of any plasticizers . .. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE) Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE) Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE) Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene .. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil 150 Mobil DTE PM Series Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | 60°F |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Specific Gravity | 0.888 g/cc | 0.888 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil 150 Mobil DTE PM Series Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona.. |