Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | ISO 1183, A |
S&E Specialty Polymers XP44-11-1 PVC Description: PVC expandable core extrusion molding compound.Application: Body side molding extruded expandable core which meets GMP.PVC.006 and Chrysler MSDC 543Information provided by S&E Specialty.. |
|||
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe EP CP 201 Cellulose Paper Reinforced Epoxy Resin - Sheet Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information .. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 33 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Very coarse weave ( |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 34 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF .. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 42 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity. Lower mechanical and electrical properties than PF CP 41.Information.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 31 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Fine weave (>30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 31 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 15880-02 Wire & Cable Flexible PVC TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 2153A Wire & Cable Flexible PVC THHN-THWN; in circuit sizes (14 AWG and larger). UL recognized for THHN, THW, THWN, TW, Oil resistant I.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8630 Moldings & Extrusions Flexible PVC Extrusion compound recommended for extruded shapes and other applications where a matte finish is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8803 Moldings & Extrusions Flexible PVC Microbe resistant extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets. Good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Ax.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 10756 Wire & Cable Flexible PVC General purpose, non-lead stabilized jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 2192 Wire & Cable Flexible PVC Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom VN-051090 PVC Compound Compuestos Dominicanos SA manufactures polycom VN product series for the extrusion of printable sheets and banners providing excellent stability, ease of processing and excellent printable character.. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 43 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical applications and low-voltage electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.35 - 1.40 g/cc | 1.35 - 1.40 g/cc | ASTM D792 |
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.34 - 1.40 g/cc | 1.34 - 1.40 g/cc | ASTM D 792 |
Karina 900D10/120-IS-PO White PVC Compound PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |