Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 - 1.35 g/cc | 1.33 - 1.35 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET F096H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Specific Gravity | 1.33 - 1.35 g/cc | 1.33 - 1.35 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET F096HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Gravity | 1.33 - 1.35 g/cc | 1.33 - 1.35 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | NBR NM-IEC 60811-1-3 |
Karina SDB 40/1-HSF Ivory PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.35 g/cc @Thickness 1.57 mm |
1.30 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP602 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne.. |
|||
Specific Gravity | 1.30 - 1.35 g/cc @Thickness 1.57 mm |
1.30 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 36/19-FC-LMP (SDB) Brown Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 752-12/6-Y-BZ Ruby Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 800-DA-10/1-A-AT-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 805-18/105-IS-SD Gray PVC Compound Packaging Grade PVCInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 822-IS-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.25 - 1.35 g/cc | 1.25 - 1.35 g/cc | ASTM D 792 |
Karina CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles and general purpose injected articles (whose temperature of use do not exceed 40°C).Information provided by Karina Indústria e Comércio de Plá.. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina E 105908-35/1-C-IS-LMP Ivory PVC Compound PVC compound recommended for extrusion of wires TW and THW.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina E 76/205-IS-SD-TR Crystal PVC Compound Crystal PVC compound recommended for sleeves.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina E 800D10/7-A-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina E 802-IS-SD Clear PVC Compound PVC compound developed for films (non-toxic).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 800D10/7-A-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina E 700-08/166-B Beige PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.15 - 1.35 g/cc | 1.15 - 1.35 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Fine weave (>30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.15 - 1.35 g/cc | 1.15 - 1.35 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 22 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Coarse weave (18-30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.15 - 1.35 g/cc | 1.15 - 1.35 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Very coarse weave ( |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 14630 Wire & Cable Flexible PVC Semi-rigid, flame retardant jacketing compound recommended. Also suitable for semi-rigid molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 15640 Wire & Cable Flexible PVC Semi-rigid UL style #1061.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 8802 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 19810 Wire & Cable Flexible PVC Primary insulation also recommended for 105°C molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 19920 Wire & Cable Flexible PVC Non-lead stabilized 105°C insulation compound recommended for THHN-THWN circuit sizes. Well suited for 105°C; 1/64 wall in all AWG sizes. CSA approved for FT1 TWN75, TEW and AWM IA constructions.. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 54915 Moldings & Extrusions Flexible PVC Medium durometer injection molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 8741 Moldings & Extrusions Flexible PVC A low gravity general purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 8863 Moldings & Extrusions Flexible PVC A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles and tubings. Meets the requirements for LP Gas hose per UL21.Information provided by Georgia .. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom BD-220699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |