Axiall 8802 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8802 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.007343 GPa
1.065 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F