| Category | Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) |
| Manufacturer | Pearl Engineering Polymers Limited |
| Trade Name | PEPLPET |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Pearl Engineering PEPLPET F097HA Film Grade Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 - 1.35 g/cc | 1.33 - 1.35 g/cc | PEPL-10-W-21 |
| Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | PEPL-10-W-67 |
| Bead Size | 2.80 mm | 0.110 in | chip size, length; PEPL-10-W-71 |
| 3.10 mm | 0.122 in | chip size, D2; PEPL-10-W-71 | |
| 3.80 mm | 0.150 in | chip size, D1; PEPL-10-W-71 | |
| Viscosity Measurement | 0.62 - 0.66 | 0.62 - 0.66 | intrinsic, [dl/gm]; PEPL-10-W-15 |
| Molecular Weight | 18500 g/mol | 18500 g/mol | Number average M |
| 37000 g/mol | 37000 g/mol | Weight average M | |
| Ash | 0.025 % | 0.025 % | PEPL-10-W-66 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | <= 65.0 J/g | <= 28.0 BTU/lb | Density at 1.38 g/cc |
| Specific Heat Capacity | 1.10 J/g-°C @Temperature 20.0 °C |
0.263 BTU/lb-°F @Temperature 68.0 °F |
|
| 1.37 J/g-°C @Temperature 80.0 °C |
0.327 BTU/lb-°F @Temperature 176 °F |
||
| 1.44 J/g-°C @Temperature 100 °C |
0.344 BTU/lb-°F @Temperature 212 °F |
||
| 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
||
| 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
||
| Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
| 0.242 W/m-K @Temperature 20.0 °C |
1.68 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
solid | |
| Melting Point | 254 - 256 °C | 489 - 493 °F | PEPL-10-W-19 |
| Maximum Service Temperature, Air | <= 70.0 °C | <= 158 °F | |
| Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
| Flash Point | 480 °C | 896 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | |
| Dielectric Constant | 3.3 | 3.3 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.20 % | <= 0.20 % | when packed; PEPL-10-W-13 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Anti-Blocking Agent (%) | 0.2 | PEPL-10-W-72 |
| Chips per Gram | 31-35 | PEPL-10-W-13 |
| COOH end groups (mval/kg) | <30 | PEPL-10-W-16 |
| Fines (ppm) | <100 | PEPL-10-W-65 |