| Category | Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) | 
| Manufacturer | Pearl Engineering Polymers Limited | 
| Trade Name | PEPLPET | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Pearl Engineering PEPLPET F096HA Film Grade Resin.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.33 - 1.35 g/cc | 1.33 - 1.35 g/cc | PEPL-10-W-21 | 
| Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | PEPL-10-W-67 | 
| Bead Size | 2.80 mm | 0.110 in | chip size, length; PEPL-10-W-71 | 
| 3.10 mm | 0.122 in | chip size, D2; PEPL-10-W-71 | |
| 3.80 mm | 0.150 in | chip size, D1; PEPL-10-W-71 | |
| Viscosity Measurement | 0.60 - 0.64 | 0.60 - 0.64 | intrinsic, [dl/gm]; PEPL-10-W-15 | 
| Molecular Weight | 17500 g/mol | 17500 g/mol | Number average M | 
| 35000 g/mol | 35000 g/mol | Weight average M | |
| Ash | 0.025 % | 0.025 % | PEPL-10-W-66 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Heat of Fusion | <= 65.0 J/g | <= 28.0 BTU/lb | Density at 1.38 g/cc | 
| Specific Heat Capacity |           1.10           J/g-°C           @Temperature 20.0 °C  | 
                  0.263           BTU/lb-°F           @Temperature 68.0 °F  | 
        |
|           1.37           J/g-°C           @Temperature 80.0 °C  | 
                  0.327           BTU/lb-°F           @Temperature 176 °F  | 
        ||
|           1.44           J/g-°C           @Temperature 100 °C  | 
                  0.344           BTU/lb-°F           @Temperature 212 °F  | 
        ||
|           1.82           J/g-°C           @Temperature 200 °C  | 
                  0.435           BTU/lb-°F           @Temperature 392 °F  | 
        ||
|           2.05           J/g-°C           @Temperature 280 °C  | 
                  0.490           BTU/lb-°F           @Temperature 536 °F  | 
        ||
| Thermal Conductivity |           0.213           W/m-K           @Temperature 280 °C  | 
                  1.48           BTU-in/hr-ft²-°F           @Temperature 536 °F  | 
        liquid | 
|           0.242           W/m-K           @Temperature 20.0 °C  | 
                  1.68           BTU-in/hr-ft²-°F           @Temperature 68.0 °F  | 
        solid | |
| Melting Point | 254 - 256 °C | 489 - 493 °F | PEPL-10-W-19 | 
| Maximum Service Temperature, Air | <= 70.0 °C | <= 158 °F | |
| Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 | 
| Flash Point | 480 °C | 896 °F | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Electrical Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | |
| Dielectric Constant | 3.3 | 3.3 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Moisture Content | <= 0.20 % | <= 0.20 % | when packed; PEPL-10-W-13 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Anti-Blocking Agent (%) | 0.2 | PEPL-10-W-72 | 
| Chips per Gram | 31-35 | PEPL-10-W-13 | 
| COOH end groups (mval/kg) | <30 | PEPL-10-W-16 | 
| Fines (ppm) | <100 | PEPL-10-W-65 |