Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-BOND® 584-29 SYRINGE-PAK™ Silver Filled Conductive Epoxy and Hardener Description: Chomerics CHO-BOND 584-29 is a two-component, highly conductive adhesive system that combines the strong adhesive characteristics of epoxy with the superior conductivity of pure silver... |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM 5537 EMI Shielding Material Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-pla.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D395 |
Parker Chomerics CHOFORM® 5550 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Specific Gravity | <= 2.20 g/cc | <= 2.20 g/cc | |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Specific Gravity | 2.20 - 2.40 g/cc | 2.20 - 2.40 g/cc | |
St. Cloud Natural Zeolite (Clinoptilolite) Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 4X08423 LNP* Thermocomp* 4X08423 is a compound based on Perfluoroalkoxy Polymer (PFA) containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D-792 |
Saint-Gobain Norton® F910 FDA Compliant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: FDA Compliant; Common in Electronics/ElectricalInformation provided by Saint Gobain Performance Products. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.002" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.003" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.005" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.010" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | Cured |
Tra-Con Tra-Bond 933-2 Moisture Resistant Chip Encapsulant TRA-BOND 933-2 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical.. |
|||
Specific Gravity | 2.20 g/cc @Temperature 25.0 °C |
2.20 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4430 KIT Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D792 |
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder White fine powder.Major Uses: Suited especially to applications requiring fine dispersion of particles. Mold lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, p.. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Daikin POLYFLON LDW-40 PTFE Low Polymer, Milky Liquid Milky liquid.Major Uses: Additive to give water repellency to water base paints.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Daikin POLYFLON L-5 PTFE Low Polymer, White Fine Powder White fine powder.Major Uses: Extreme pressure additive and lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, etc.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |
|||
Specific Gravity | 2.20 - 2.23 g/cc | 2.20 - 2.23 g/cc | ASTM D792 |
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue Information provided by Adamas, HPM |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | |
Asahi Glass Fluon® CD076 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Specific Gravity | 2.20 g/cc | 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 2.20 - 2.22 g/cc | 2.20 - 2.22 g/cc | ASTM D792 |
Adamas Adalon® 510 PTFE, 5% MoS2 Information provided by Adamas, HPM |