Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.85 g/cc | 1.85 g/cc | Slurry |
Omya OMYACARB® 3 - FL Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Employed in rubber and plastic applications such as ri.. |
|||
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ASTM D792 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM D-792 |
Glastic GLASTHERM HT220 Insulation Sheet Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM 792 |
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM 792 |
Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
BCC Products BC 7062H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |