| Category | Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC |
| Manufacturer | BMC - Bulk Molding Compounds Inc. |
| Trade Name | BMC |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Bulk Molding Compounds BMC 6605A Polyester Molding Compound.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
| Water Absorption | <= 0.10 % | <= 0.10 % | 24 hours, 23°C |
| Linear Mold Shrinkage | 0.0013 - 0.0035 cm/cm | 0.0013 - 0.0035 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Barcol | 23 - 25 | 23 - 25 | |
| Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
| Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
| Compressive Strength | 138 - 172 MPa | 20000 - 25000 psi | |
| Izod Impact, Notched | 1.60 - 2.67 J/cm | 3.00 - 5.00 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | >= 204 °C | >= 400 °F | |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.7 - 17.3 kV/mm | 400 - 440 kV/in | Short Time |
| Arc Resistance | >= 180 sec | >= 180 sec |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 104 - 138 °C | 220 - 280 °F |