Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | Part A; TM R050-16 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Specific Gravity | 1.16 g/cc @Temperature 20.0 °C |
1.16 g/cc @Temperature 68.0 °F |
|
M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative GUARD DOGâ„¢ UV531(flake or powder) light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - .. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ISO 2781 |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM 792 |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SMG 7500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 2076 Superior Black Color Concentrate, 40% Carbon Black Based In EVA DescriptionPOLYBLAK® Black 2076 is a superior black color concentrate containing 40% carbon black in EVA. This masterbatch is designed to provide good opacity and a regular blue undertone with pig.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | |
Trelleborg E850 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
DSM Biomedical CarboSil® 20 80A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU) A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | Part A |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | Part A |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D-792 |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |