Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GRECO ISOTHANE 2075A Poly(caprolactone)ester TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 2075A Poly(caprolactone)ester TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
Tensile Strength, Yield 2.90 MPa

@Strain 50.0 %
421 psi

@Strain 50.0 %
ASTM D412
5.70 MPa

@Strain 100 %
827 psi

@Strain 100 %
ASTM D412
8.30 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
Elongation at Break 630 %
630 %
ASTM D412
Tear Strength 70.0 kN/m
399 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 10
10
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
30 %

@Temperature 70.0 °C,
Time 79200 sec
30 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Users viewing this material also viewed the following: