Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.07 g/cc | 1.07 g/cc | Mixed; TM R050-16 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
PolyOne Maxxam™ PD 20 TF Black Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Polymax® Maxelast® P2775 TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | foam molded; ASTM D 792 |
SABIC Innovative Plastics Lexan® FL3000 PC Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Resinlab® RC8041 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ISO 1183 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Specific Gravity | 1.07 - 1.11 g/cc | 1.07 - 1.11 g/cc | |
LG Chemical CP-WBM Polycarboxylic Copolymer Description: CP-WRM is the main raw material for concrete admixture, which improves water reducing abilities. CP-WRM was developed through our advanced synthetic technologies, imparting good compati.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM 792 |
Multibase Multi-Flex® A 4001 LCS Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced Used in golf cart roof etc.Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Supreme Petrochem SP 562 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange 1770E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1770E is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1770E is .. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Specific Gravity | 1.07 g/cc @Temperature 25.0 °C |
1.07 g/cc @Temperature 77.0 °F |
|
Dow Corning LSPBK27 SILICONE MASTERBATCH BLACK Information provided by Dow Corning |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Diamond Polymers ASA S210 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Diamond Polymers ASA TW-15H Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat Resistance, High IzodInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | |
Esstech X-968-7048 2- Hydroxyethyl Methacrylate Direct Casting Grade, C6H10O3 HEMA is a primary alcohol making it a good adhesion promoter in anaerobic adhesives. The purity level of this methacrylate monomer also makes it cost efficient. Listed on the Toxic Substance Contro.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
C.O.I.M. LARIPUR® LPR7060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7175-1000 TPE Product Description: StarFlex P 7175-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |