Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
Radici Heraflex® A 75-21-60 TPS-SEBS Thermoplastic Elastomer TPS-SEBS Thermoplastic Elastomer. 75 Shore A.Application examples: rollersProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | TA4202B |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
LG Chemical NBR 3250 High Acrylonitrile Polymer Description: NBR 3250 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3250 is a non staining, medi.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Clean 1188 Cleaning solution Description: Cleaning solution for Indigo WS6600Usage: Michem® Clean 1188 is the recommended cleaning solution for Michem® In-Line Primer 030 priming solution. This cleaner should be added to .. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion Description: Modified ethylene acrylic acid dispersionUsage: Michem®Prime 5931 is a modified ethylene acrylic acid dispersion which provides improved adhesion to polyolefin substrates. It also ex.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific) High modulus/impact/heat PPE+PP. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning 60 PRINTERS' SOLUTION 60% active emulsion of silanol-terminated polydimethylsiloxane fluid.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning 62 PRINTERS' SOLUTION 55% active emulsion of medium viscosity polydimethylsiloxane fluid; contains antistat.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® PMCP7689 Crosslinker Syl-Off® 7689 Crosslinker is a solvent-free silicone crosslinker for polyester substrates.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
Dow Corning 1665 EMULSION Dow Corning® 1665 Emulsion is a milky white cationic emulsion of an intermediate viscosity polydimethylsiloxane fluid. The emulsion contains 55% silicone and has a relatively low particle size.Info.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited.. |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning 36 EMULSION Non-ionic, 35% active, emulsion of a medium viscosity trimethylsilyl terminated polydimethylsiloxane. This product has been replaced by Dow Corning® IE 39 EmulsionInformation provided by Dow Cornin.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D471; ISO 2781 |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D471 |
Advanced Polymer Alloys DuraGrip™ 6830 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D471 |
Advanced Polymer Alloys DuraGrip™ 6840 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |