Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 23/23°C; ASTM D792 |
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 23/23°C; ASTM D792 |
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.980 - 1.02 g/cc | 0.980 - 1.02 g/cc | ASTM D792 |
S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Radici Heraflex® B 35D 11 I SL 250 Styrenic Thermoplastic Elastomer SBS Shore hardness: 35D (3s)Exceptional resistance to abrasion and flex fatigue, as well as mechanical performanceApplication examples: winter footwearInformation provided by Radici group. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Radici Heraflex® HA 60-22-60 TPS-SEBS Thermoplastic Elastomer TPS-SEBS Thermoplastic Elastomer. 60 Shore A. Good adhesion on PA6.Application examples: Soft touch grip for power toolsProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 23°C; ASTM D792 |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 52137 as an additive, provides lubricity and is effective as a high temperature mold release for metal dies.We serve many market.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Emulsion 65140 Nonionic polypropylene emulsion Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 65140 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is n.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Flex P1883 Water based heat seal coating and primer Description: Water based heat seal coating and primer for extrusion coated resins.Usage: Michem® Flex P1883 is a general purpose primer for metal and paper substrates to promote adhesion to extru.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4990R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Shield 251 Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Shield 251 is an additive which provides abrasion resistance in coatings formulations. Michem® Shield 251 has proven most effective in.. |
|||
Specific Gravity | 0.980 - 1.02 g/cc | 0.980 - 1.02 g/cc | |
Michelman® Sapphire 5.0 Ink Primer Primer for use with HP Indigo press.Q4310A (Sapphire 5.0) is designed as a primer for HP Indigo substrates to render them compatible to ink. It can be used on paper substrates.Q4310A (Sapphire 5.0) .. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | True |
Shin-Etsu Silicones KSP-101 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1052-30 Nitrile Elastomer Nipol 1052-30 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Low Mooney versi.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 33-5SR Nitrile Elastomer Special-purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.Special purpos.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Zealloy® 1422X14 Modifier for Thermoplastics Zealloy 1422X14 is a copolymer of butadiene and acrylonitrile of medium-high oil resistance. It is furnished as particulate rubber approximately particle size 16-18 mesh. Sufficient antioxidant is .. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105-E is a general purpose erucamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF.. |
|||
Specific Gravity | 0.980 g/cc @Temperature 25.0 °C |
0.980 g/cc @Temperature 77.0 °F |
|
Dow Corning 9506 Powder A spherical white powder comprised of dimethicone / vinyl dimethicone crosspolymer for use in skincare, suncare, and color cosmetic applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.980 g/cc @Temperature 25.0 °C |
0.980 g/cc @Temperature 77.0 °F |
|
Dow Corning AP-8087 FLUID This amino functional siloxane polymer can be used in a range of hair care applications including shampoos, rinse-off conditioners, leave-in conditioning treatments, colorants, and styling products... |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Esstech X-724-0000 Isobornyl Methacrylate, C14H22O2 The cyclic group of isobornyl methacrylate allows it to react in free radical polymerization while also acting as an excellent diluent. Listed on the Toxic Substance Control Act List. CAS # 7534-9.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFIPP 2010 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® DN1201L Terpolymer Elastomer Nipol DN1201L is a low-temperature polymerized terpolymer of acrylonitrile, butadiene and isoprene. This polymer is intended to give better physical and processing characteristics than a regular nit.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® DN3380 Nitrile Elastomer Nipol DN3380 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Low mold fouling, fast curing .. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® NX775 Carboxylated Nitrile Elastomer Nipol NX775 is a cold polymerized, butadiene-acrylonitrile-carboxylic acid terpolymer. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent process.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ISO 2782 |
AlphaGary Evoprene™ HP 3730 High Performance Thermoplastic Elastomer Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP.. |