Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 52137 as an additive, provides lubricity and is effective as a high temperature mold release for metal dies.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 62.5 - 63.5 %
62.5 - 63.5 %
pH 2.0 - 12
2.0 - 12
Recommended pH of system
8.5 - 9.5
8.5 - 9.5
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance Light yellow, translucent liquid
Emulsifier Charge Nonionic
Solids Type Polyethylene