Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Michelman®
Trade Name Michem® Prime
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4990R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent resistance of coatings and adhesives. Michem® Prime 4990R can serve as a tie coat or primer for extrusion coatings, a foil laminate, a specialty paper coating, a paper sizing agent, a heat sealable coating or a nonwoven binder.When manufactured in the USA and Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted) Germany: BfR Recommendation XIV (Restricted)and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in the USA, Belgium and Signapore: FDA:175.105: Components of adhesives175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 65 - 68 %
65 - 68 %
pH >= 7.0
>= 7.0
Recommended pH of system
7.8 - 8.8
7.8 - 8.8
Brookfield Viscosity 200 - 850 cP
200 - 850 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Ammoniated dispersion
Solids Type Ethylene Acrylic Acid Copolymer