Michelman® Michem® Emulsion 65140 Nonionic polypropylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 65140 Nonionic polypropylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 65140 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is needed.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in the USA: FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 59.5 - 60.5 %
59.5 - 60.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
7.7 - 9.0
7.7 - 9.0
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance Amber, translucent liquid
Emulsifier Charge Nonionic
Solids Type Meleated Polypropylene