Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Flexirene® MS 20 A Linear Low Density Polyethylene Flexirene MS 20 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 A are characterized by optimum low tempe.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. F.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505 |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505 |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505 |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Specific Gravity | 0.921 - 0.925 g/cc | 0.921 - 0.925 g/cc | ASTM D1505 |
LG Chemical SEETEC BF315 LDPE Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505 |
LG Chemical LUTENE FB0800 LDPE Blown Film Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183-D |
LG Chemical LUTENE XL8080TR PE Compound Description: LUTENE XL8080TR has excellent electrical properties for medium and high voltage power cable insulation and especially it shows improved water tree resistance and has thermal aging prope.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ISO 1183 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil EAL 224H Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil EAL 224H Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr.. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem EB861 Blown Film Extrusion Low Density Polyethylene Medium-resistance films for general use; Mulching films; Shrink films; Coextrusion.Information provided by Braskem. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem F0421D Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem PB682 Blow Molding Low Density Polyethylene Blow molding; Injection blow molding; Medium resistance mechanical film; Expanded PE blankets.Information provided by Braskem. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem BF2021 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Specific Gravity | 0.921 g/cc | 0.921 g/cc | ASTM D1505/D792 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |