Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D1505 |
I. Stern 3335 Prime Impact Copolymer Polypropylene Features:Superior color and process stabilityLow odor, good flow and set up behaviorExcellent see through clarityApplicationsReusable food containersHousewaresPackagingInformation provided by I. Ste.. |
|||
Specific Gravity | 0.900 - 0.920 g/cc | 0.900 - 0.920 g/cc | |
Michelman® Michem® Dispersion 471 Solvent dispersion of carnauba wax Description: Solvent dispersion of carnauba waxUsage: Michem® Dispersion 471 provides slip and abrasion resistance. This product has proven very effective for slip and abrasion resistance when us.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ISO 1183 |
MRC Polymers MAXTEL™ 620-BK Polypropylene Copolymer • For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer Notes: Water; Clear; Adhesion to Polycarbonate Features: High Coefficient of FrictionInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | +/- 0.02; ASTM D792 |
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Specific Gravity | 0.900 - 0.920 g/cc | 0.900 - 0.920 g/cc | |
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color con.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | |
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | Mixed |
Tra-Con Tra-Bond FDA16 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-16 EPOXY ADHESIVE is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests,.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-001 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc @Temperature 25.0 °C |
0.900 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 23-30% COATING Syl-Off® 23 Paper Coating 30 Percent is a 30% active solids dispersion of silanol functional silicone polymers and multifunctional crosslinkers in xylene.Information provided by Dow Corning |
|||
Specific Gravity | 0.900 g/cc @Temperature 25.0 °C |
0.900 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® SB 7458 COATING Base polymer component for Syl-Off® brand solvent-based, platinum-catalyzed silicone release coatingsInformation provided by Dow Corning |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | DIN-53479 |
Dynasol Solprene® 200 Polybutadiene Rubber Solprene 200 is a medium cis polybutadiene with excellent mixing and processing behavior. It is used as ingredient in tire compounds and in other applications where good performance at low temperatu.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
PolyOne Synprene® RT-3860MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
PolyOne Synprene® IT 38-046E Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:FDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A thermoplastic.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
PolyOne Synprene® ST-6160 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |