PolyOne Synprene® IT 38-046E Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® IT 38-046E Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:FDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. PLEASE CONTACT US TO REVIEW THE SUITABILITY OF SPECIFIC PRODUCTS IN SPECIFIC APPLICATIONS. This statement is only an overview of the FDA listings for this product. IT IS THE CUSTOMER'S RESPONSIBILITY TO ENSURE THAT THE COMPOUND IS SUITABLE FOR ITS INTENDED APPLICATIONS.Information provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
Instant; ASTM D2240
Tensile Strength, Yield 5.86 MPa
850 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
3.65 MPa

@Strain 300 %
530 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 750 %
750 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 21.0 kN/m
120 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 15 %
15 %
Method B, 73°F(23°C), 22 hrs; ASTM D395