Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dynasol Solprene® 200 Polybutadiene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dynasol
Trade Name Solprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 200 Polybutadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solprene 200 is a medium cis polybutadiene with excellent mixing and processing behavior. It is used as ingredient in tire compounds and in other applications where good performance at low temperatures, excellent abrasion resistance, low heat build-up and good dynamic fatigue resistance are needed. It is packed in bales wrapped in low melting point polyethylene film.Applications:TiresIndustrial goodsInformation provided by Dynasol
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
DIN-53479
Volatiles <= 0.75 %
<= 0.75 %
ASTM D-5668
Mooney Viscosity 49

@Temperature 100 °C
49

@Temperature 212 °F
ML (1 + 4); ASTM D-1646
Ash <= 0.20 %
<= 0.20 %
ASTM D-1416
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -92.0 °C
-134 °F
NM 300-58
Chemical Properties Metric English Comments
Acid Value <= 0.030
<= 0.030
organic acid %; ASTM D-1416
Descriptive Properties Value Comments
Color Alpha, max 15
Free Soap, % max 0.03
Users viewing this material also viewed the following: