Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® RT-3860MS Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Synprene® RT-3860MS Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Instant; ASTM D2240
61
61
Instant; ASTM D2240
Tensile Strength, Yield 5.72 MPa
830 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
5.72 MPa
830 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
3.79 MPa

@Strain 300 %
550 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 620 %
620 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
620 %
620 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 50 %
50 %
Bayshore; ASTM D2632
Tear Strength 35.1 kN/m
200 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
ASTM D746