Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.025 cm/cm | 0.020 - 0.025 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/05T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.025 cm/cm | 0.021 - 0.025 in/in | ASTM D955 |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Linear Mold Shrinkage, Flow | 0.0215 - 0.025 cm/cm | 0.0215 - 0.025 in/in | |
LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.025 cm/cm @Time 86400 sec |
0.019 - 0.025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm @Time 86400 sec |
0.015 - 0.025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm @Time 86400 sec |
0.015 - 0.025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T102 PET, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.023 - 0.025 cm/cm @Time 86400 sec |
0.023 - 0.025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF R1000JX4 PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for .. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm @Time 86400 sec |
0.015 - 0.025 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for .. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |