Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.18 mm |
0.012 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 1.00 mm |
0.012 in/in @Thickness 0.0394 in |
|
Kuraray Genestarâ„¢ TA104 Nylon Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-220 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-240 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-340 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific) LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionTPCI# 9586102Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
|
Toyobo ECOVYLOPET® EMC2301E PET Bottle Recycling Grade, 15% Filler Reinforced Features: PET Bottle Recycling Grade, 15% Filler Reinforced, Modified TypeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.022 cm/cm | 0.012 - 0.022 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSS/2 FA PA666 Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow .. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 4.00 mm |
0.012 - 0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
Clariant PA223 Nylon 6, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |