Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber PA 6, injection molding grade, 30% reinforced (glass fibers + carbon fibers), conductive, intrinsic color black, good heat-ageing resistance |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 294-4, 2577 |
Lanxess Pocan® KU 2-7205 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | Sim. To ISO 294-4 |
DSM Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Linear Mold Shrinkage, Flow | 0.0021 cm/cm | 0.0021 in/in | ISO 2577 |
BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |