Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | 150x105x3, 260°C / MT 80°C; 500 bar; acc. ISO 2577 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 3.17 mm |
0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MB006SU is a compound based on Polypropylene resin containing Glass Bead. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performanc.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 588P NC010 Acetal (POM) Nucleated Medium Viscosity Acetal HomopolymerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.021 cm/cm @Time 86400 sec |
0.019 - 0.021 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 75 A.1 TPE-S, Shore A70, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 60 HT A.01 black TPE-S, Shore A60, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | Sheet; ISO 294 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications .. |