Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
PolyOne Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Time 86400 sec |
0.012 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.18 mm |
0.012 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® PA6/6 IM C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6 FR-N Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionTPCI# 9586102Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler/Unspecified FillerReinfor.Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.021 cm/cm @Thickness 3.20 mm |
0.012 - 0.021 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm @Thickness 3.20 mm |
0.012 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific) PA6 based unfilled GTX for Wheel cover |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
|
Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.20 mm |
0.012 in/in @Thickness 0.126 in |
|
Unitika EX-1030 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | DIS 294-4 |
Wellman Wellamid® 42L-XE-N Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.022 cm/cm | 0.012 - 0.022 in/in | |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Diameter 2.00 mm |
0.012 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Linear Mold Shrinkage, Flow | 0.012 cm/cm @Thickness 3.20 mm |
0.012 in/in @Thickness 0.126 in |
|
Unitika EX-1222 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |