Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne Maxxam™ FR MF5210-0301 DK GRAY 2451 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ MD 4245-59770 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 6500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | 60x60x2; 250°C / WZ 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON MX01767C PP LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 CF10 TS15 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(13%) and Silicone Lubricant(2%)Features: Lubricated Appearance: BlackInforma.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Time 86400 sec |
0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
|
Unitika A1030SR PA6, Dry Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ISO 294-4 |
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced PEEKInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | |
Ineos ABS Triax® 1180 ABS + Polyamide Blend (DAM)
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business r.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |