Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.015 - 0.050 cm/cm | 0.015 - 0.050 in/in | |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | ASTM D955 |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | ASTM D955 |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON F-201 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON F-302 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by .. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into .. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder 20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder 15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder 30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder 15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder 25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Linear Mold Shrinkage | 0.010 - 0.050 cm/cm | 0.010 - 0.050 in/in | 0.125 in; ASTM D955 |
Entec Hypel® PELD20/.920 LDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | ASTM D955 |
Ex-Tech Plastics VersaTech™ APET Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder 25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | ASTM D955 |
Alcoa KAMA 4203 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |