Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KLZ Nylon 6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 W Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | |
SABIC PP 651H Polypropylene Random Copolymer for PIPE Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App.. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm | 0.018 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 D-S10 Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, increased dry impact resistance (for dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm @Thickness 3.17 mm |
0.020 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acctuf® 3143 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Sheet extrusion; Thick-wall Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injectio.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm | 0.018 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 80-8387 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.025 cm/cm | 0.0080 - 0.025 in/in | ASTM D955 |
Cheng Yu Plastic 3235 TPE Rubber |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Accpro® 9433 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical app.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Accpro® 9965 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |