Material Notes:
Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical Applications: PP 651H can be used for hot & cold water pipes & fittings.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.897 g/cc
0.0324 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM D790A
Izod Impact, Notched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 135 °C
275 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 200 - 230 °C
392 - 446 °F
Barrel Temperature
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F