Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z805P Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYform POM C M90 K5 Polyoxymethylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis MG9621S Polyethylene MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic NG1400S Nylon 66, 40% Glass Fiber Reinforced |
|||
Linear Mold Shrinkage | 0.0050 - 0.020 cm/cm | 0.0050 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic T881 Flame Retardant PBT |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 422451S SBS Based Material, 45D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic FV3010 Polyformaldehyde |
|||
Linear Mold Shrinkage | 0.013 - 0.020 cm/cm | 0.013 - 0.020 in/in | Dry; ASTM D2863 |
Asahi Kasei Leona® 1700S Nylon 66 Similar to 1500 but with even higher molecular weight. Suitable for extrusion of thick-wall parts.Applications:Rods, films Information provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |