Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.0140 cm/cm | 0.00200 - 0.0140 in/in | Average value: 0.00530 cm/cm Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0140 cm/cm | 0.00300 - 0.0140 in/in | Average value: 0.00582 cm/cm Grade Count:27 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00636 cm/cm Grade Count:17 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0140 cm/cm | 0.000500 - 0.0140 in/in | Average value: 0.00563 cm/cm Grade Count:669 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00560 - 0.0140 cm/cm | 0.00560 - 0.0140 in/in | Average value: 0.00908 cm/cm Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0140 cm/cm | 0.000100 - 0.0140 in/in | Average value: 0.00727 cm/cm Grade Count:51 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0140 cm/cm | 0.000400 - 0.0140 in/in | Average value: 0.00826 cm/cm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00255 cm/cm Grade Count:53 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0140 cm/cm | 0.000500 - 0.0140 in/in | Average value: 0.00686 cm/cm Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00485 cm/cm Grade Count:13 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00631 cm/cm Grade Count:12 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0140 cm/cm | 0.00400 - 0.0140 in/in | Average value: 0.00857 cm/cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |