Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.994 - 1.24 g/cc
0.0359 - 0.0448 lb/in³
Average value: 1.08 g/cc Grade Count:7
Linear Mold Shrinkage 0.00560 - 0.0140 cm/cm
0.00560 - 0.0140 in/in
Average value: 0.00908 cm/cm Grade Count:5
Melt Flow 0.100 - 23.6 g/10 min
0.100 - 23.6 g/10 min
Average value: 4.69 g/10 min Grade Count:6
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.0 - 23.1 MPa
2180 - 3350 psi
Average value: 17.3 MPa Grade Count:4
Tensile Strength, Yield 15.0 - 33.9 MPa
2180 - 4920 psi
Average value: 19.1 MPa Grade Count:6
Elongation at Break 0.790 - 15.0 %
0.790 - 15.0 %
Average value: 7.06 % Grade Count:7
Modulus of Elasticity 1.70 - 4.86 GPa
247 - 705 ksi
Average value: 3.21 GPa Grade Count:6
Flexural Yield Strength 29.8 - 43.0 MPa
4320 - 6240 psi
Average value: 34.5 MPa Grade Count:6
Flexural Modulus 1.12 - 4.10 GPa
163 - 595 ksi
Average value: 2.05 GPa Grade Count:6
Izod Impact, Notched 0.210 - 0.430 J/cm
0.393 - 0.806 ft-lb/in
Average value: 0.310 J/cm Grade Count:4
Izod Impact, Unnotched 0.270 - 2.40 J/cm
0.506 - 4.50 ft-lb/in
Average value: 1.11 J/cm Grade Count:5
Thermal Properties Metric English Comments
CTE, linear 36.0 - 99.0 µm/m-°C
20.0 - 55.0 µin/in-°F
Average value: 64.3 µm/m-°C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 62.0 °C
109 - 144 °F
Average value: 50.4 °C Grade Count:5
Flammability, UL94 HB
HB
Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 200 °C
392 °F
Average value: 200 °C Grade Count:5