Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0090 cm/cm | 0.0030 - 0.0090 in/in | ASTM D955 |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Kolon SPELLOY® KB133G15 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm @Temperature 121 °C, Time 3600 sec |
0.0070 - 0.0090 in/in @Temperature 250 °F, Time 1.00 hour |
48 hours after molding; ISO 294-3/4 |
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | as molded; ISO 294 |
Solvay Engineered Polymers SEQUEL® 1718HF Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1718HF engineered polyolefin is designed for painted automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.0090 cm/cm | 0.0080 - 0.0090 in/in | ASTM D955 |
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm @Temperature 23.0 °C |
0.0060 - 0.0090 in/in @Temperature 73.4 °F |
Plumb; ASTM D955 |
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Samyang Tramid® 210G15 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0050 - 0.0090 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO 294-4 |
Wellman Wellamid® GF13-66 22LH-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0050 - 0.0090 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | D955 |
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | Flow direction; ASTM D955 |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
Ecomass® 1850ZC84 Stainless Steel Powder Filled Polyamide (PA6), Injection Molding Stainless Steel Powder Filled Polyamide (PA6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | Bayer Test |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0090 cm/cm | 0.0030 - 0.0090 in/in | ASTM D955 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.0075 - 0.0090 cm/cm | 0.0075 - 0.0090 in/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |