Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D-955 |
Plaskolite Optix® CA - 900 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Gichem GILAC F120 Acrylonitrile Butadiene Styrene
(discontinued **) ABS high fluidity, good stiffness and excellent stampability. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Gichem GILAC G160 Acrylonitrile Butadiene Styrene
(discontinued **) ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Temperature 23.0 °C |
0.0040 - 0.0060 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM-D955 |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
LTL Color Compounds ColorRxâ„¢ ABS-0502AF Food Grade ABS A high gloss, injection molding grade of ABS with FDA food contact approval, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Temperature 23.0 °C |
0.0040 - 0.0060 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/BK Polyamide 66, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | Compression Molding. ASTM D955 |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D 955 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Diamond Polymers ABS 9500P Injection Molding Grade, Ultra High Impact Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Diamond Polymers ASA/PC 7030 Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D-955 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0010 - 0.0060 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |