Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYshine PBT D221 PBT, Impact Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications Bormed HF855MO is a high modulus polypropylene homopolymer and is especially developed within the proprietary Borstar technology. Bormed HF855MO combines an unique balance of properties for high sp.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding BorPure™ MB6561 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic PP231H TALC 40 Polypropylene, 40% Talc, High Heat |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic FR200GV45 Flame Retardant Nylon 66, 45% Glass Fiber |
|||
Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic FR200N Flame Retardant Nylon 66 |
|||
Linear Mold Shrinkage | 0.013 - 0.020 cm/cm | 0.013 - 0.020 in/in | Dry; ASTM D2863 |
Asahi Kasei Leona® FR200 Nylon 66 UL94 V-0; halogen-free and phosphor-free.Applications:Connectors, switches, and other electrical and electronic parts Information provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.0040 - 0.020 cm/cm | 0.0040 - 0.020 in/in | ASTM D955 |
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm @Thickness 3.17 mm |
0.010 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |