Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0020 - 0.0070 cm/cm | 0.0020 - 0.0070 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Temperature 23.0 °C |
0.0050 - 0.0070 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa JH820 Modified PC Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Temperature 23.0 °C |
0.0050 - 0.0070 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM-D955 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Thickness 4.00 mm |
0.0050 - 0.0070 in/in @Thickness 0.157 in |
|
Teijin Panlite® L-1225ZL100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is a thin wall injection molding grade as it has high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear color.Applications:.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ISO 294-4 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
PlastxWorld CEVIAN® E81 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0070 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
Total PSI 8350 (AS) High Impact Polystyrene Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
Ineos Nova 1301 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |