Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000400 - 0.00300 cm/cm | 0.000400 - 0.00300 in/in | Average value: 0.00157 cm/cm Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00300 cm/cm | 0.000500 - 0.00300 in/in | Average value: 0.00183 cm/cm Grade Count:9 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00300 cm/cm | 0.00200 - 0.00300 in/in | Average value: 0.00269 cm/cm Grade Count:8 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00300 cm/cm | 0.00200 - 0.00300 in/in | Average value: 0.00267 cm/cm Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00300 cm/cm | 0.000500 - 0.00300 in/in | Average value: 0.00146 cm/cm Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00300 cm/cm | 0.000100 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00300 cm/cm | 0.000500 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:21 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00300 cm/cm | 0.00100 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00300 cm/cm | 0.000 - 0.00300 in/in | Average value: 0.00100 cm/cm Grade Count:19 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00250 - 0.00300 cm/cm | 0.00250 - 0.00300 in/in | Average value: 0.00275 cm/cm Grade Count:10 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00300 cm/cm | 0.00150 - 0.00300 in/in | Average value: 0.00213 cm/cm Grade Count:6 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00300 cm/cm @Temperature 80.0 - 80.0 °C |
0.00300 - 0.00300 in/in @Temperature 176 - 176 °F |
Average value: 0.00300 cm/cm Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00300 cm/cm | 0.000500 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00300 cm/cm | 0.00100 - 0.00300 in/in | Average value: 0.00221 cm/cm Grade Count:9 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |