Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 4.00 mm |
0.015 - 0.025 in/in @Thickness 0.157 in |
10.0 mm wide molded rod; ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Linear Mold Shrinkage | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
Flow; DAM |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® NSB 90 NT Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
Kolon SPESIN® KP513 PBT Alloy Resin Excellent extrudable and SpinningApplications: Mono filamentInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 5521 BLK TPE A 5521 is based on Shell's Kraton technology licensed to Multibase. The product is extensively used in automotive and non-automotive applications. Multi-Flex TPE contains Kraton™ G.Data p.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Multibase Multi-Flex® A 7011 TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 2.00 mm |
0.015 in/in @Thickness 0.0787 in |
|
Toyobo PELPRENE™ S3001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene PP copolymer extrusion gradeFlame retardant class V2, PBDE free, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Ashley Polymers Ashlene® 520 Nylon 66 A general purpose basic Nylon 66 resin, slightly lubricated.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Ashley Polymers Ashlene® 737 Nylon 6 A modified nylon for applications requiring exceptional flexibility for extrusion.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP 1245A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |