Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 49 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM D955 |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM D955 |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm @Thickness 3.17 mm |
0.0065 in/in @Thickness 0.125 in |
ASTM D995 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | STN EN ISO 294-4 |
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM D955 |
LyondellBasell Sequel® 1718 Engineered Polyolefin Data provided by Solvay Engineered Polymers.An engineered polyolefin designed for exterior painted automotive applications requiring dimensional stability over a broad temperature range. This mater.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM Data; MD |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM Data; MD |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM Data; MD |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Styron Pulse® B250 ABS + Polycarbonate PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. .. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM D955 |
Styron Pulse® B-270 PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | mold average;Borealis Method |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | mold average;Borealis Method |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm @Thickness 3.17 mm |
0.0065 in/in @Thickness 0.125 in |
ASTM D955 |
Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Cytec EN-2534 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | Flow Direction; ASTM D955 |
Diamond Polymers SBS 1001 Styrene Butadiene Block Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | |
BASF Ultramid® B3K PA6 (Conditioned) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | restricted |
BASF Ultramid® B3L BK00464 PA6 (Conditioned) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | restricted |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | Transfer; ASTM D955 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | ASTM D955 |
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | restricted |
BASF Ultramid® B3K BK00464 PA6 (Conditioned) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | restricted |
BASF Ultramid® B3L BK00464 PA6 (Dry) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM D955 |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | mold average; Borealis Method |
Borealis Daplen™ EF209AE Polypropylene TPO Compound Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |