Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 051.LJ Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Slip Level | 500 ppm | 500 ppm | erucamide; Borealis Method |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Slip Level | 500 ppm | 500 ppm | Additive - Erucamide |
Borealis Himod™ FT7294 LDPE for Film Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
Slip Level | 500 ppm | 500 ppm | |
ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |