Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 40 - 70 µm | 40 - 70 µm | d50 |
Magyar Aluminum ALO-DFC Alumina Alumina for Polishing |
|||
Particle Size | 40 - 80 µm | 40 - 80 µm | d50 |
Magyar Aluminum ALOLT 01 Aluminum Hydroxide Dry type |
|||
Particle Size | 40 - 60 µm | 40 - 60 µm | |
Lucite International Colacryl ® D150 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 40 µm | 40 µm | |
Shin-Etsu Silicones KMP-400 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 40 µm | 40 µm | |
Silberline Sparkle Silver® 3624 Sparkle Silver® 3624 is a coarse, brilliant, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a w.. |
|||
Particle Size | 40 µm | 40 µm | at a density of 2.10 g/cc |
TIMCAL TIMREX® GB98/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 40 - 51.5 µm | 40 - 51.5 µm | d90, Guaranteed |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 40 - 55 µm | 40 - 55 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 40 µm | 40 µm | D50 (Malvern) Size B |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 40 µm | 40 µm | D50 (Malvern) Size B |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 40 µm | 40 µm | Laser Method (Dry) |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Particle Size | <= 40 µm | <= 40 µm | |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Particle Size | <= 40 µm | <= 40 µm | Max |
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Size | <= 40 µm | <= 40 µm | Max |
CIMBAR BariScan Ultra Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-G15 PTFE Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-G20 PTFE Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-S15 PTFE 15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-S25 PTFE Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average D50; Laser Diffraction |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M K46 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | D50 |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Particle Size | 40 - 49 µm | 40 - 49 µm | D50, Range |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Particle Size | 40 µm | 40 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SA300S30 Silver-coated Aluminum Granules Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumIn.. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |