Azoty Tarnow™ TARFLEN SM-G15 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Azoty Tarnow™ (Zaklady Azotowe)
Trade Name TARFLEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azoty Tarnow™ TARFLEN SM-G15 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
ISO 1183
Filler Content 15 %
15 %
Graphite
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868
Ball Indentation Hardness 52.0 MPa
7540 psi
ISO 2039-1
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527
Elongation at Break 210 %
210 %
ISO 527
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 61 ohm-cm
61 ohm-cm
1mA; IEC 60093
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Molding Pressure